Beyond the CoA: The Critical Role of Residual Nickel and Atmospheric Breath in Polymer Failure

A Certificate of Analysis (CoA) is a snapshot, not a biography. In high-precision manufacturing, a batch of 12-HSA can meet every 99% purity spec and still “poison” a reactor. At Nova Industries, our deep-dive analysis has identified two “Silent Killers” of industrial batches: Residual Transition Metals and Logistics Breath.

  1. Nickel Poisoning: During the hydrogenation of castor oil to create Castor Wax, nickel catalysts are used. If the filtration process isn’t calibrated to the sub-micron level, trace nickel remains. In downstream polymerization, this trace nickel acts as a pro-oxidant, causing the final resin to “yellow” or, worse, deactivating the expensive catalysts the customer uses for their own reaction.

  2. Atmospheric Breath: Castor derivatives are hygroscopic. During a 30-day sea voyage in a standard container, temperature cycles cause the drums to “breathe,” drawing in humid marine air. For Polyurethane (PP) grade oil, a rise in moisture from 0.02% to 0.08% is enough to trigger $CO_2$ gassing in the customer’s mold, resulting in micro-voids (pinholes) that lead to structural failure.

True quality leadership means guaranteeing the Process Integrity of the supply chain, ensuring that the invisible contaminants never reach the customer’s kettle.

Scroll to Top